Obtaining Insufficient Glossiness

Reason: A surface filler at sufficient level and quality is not applied according to the surface and type of wood; incompliance of top coat or varnish with the surface filler; surface filler does not have the sufficient capacities of stiffness, filling and spreading; a low-quality and inappropriate thinner is used for top coat qualities; top coat application is not at the sufficient thickness.

Solution: Before applying top coat gloss paint or varnish, always use surface fillers of sufficient quality. High-quality thinner should be used on properly prepared surfaces and top coat should be applied with a sufficient film thickness. Sandpaper no.400-600 should be used for the surfaces you cannot obtain the sufficient glossiness and top coat paint or varnish should be applied one more time regarding the reasons above.