Spilling and Hanging

Reason: Very thick paint is applied at one time on vertical and curved surfaces; application viscosity of paint is very low, paint gun is held at various angles different from a steep angle to the surface or in different ways, so paint and varnish accumulate at one paint.

Solution: Paint and varnish viscosity should be regarded; application should be carried out as thin coats especially on vertical surfaces; distance between paint gun and surface should be 20cm for normal operations and 30cm for high pressed operations. In such cases, sanding operating should be carried out on these problematic surfaces very well using sandpaper no. 400-600 and paint should be applied as one coat one more time regarding the reasons causing the problem.